royhall:
I also use, honda4.nl I find them very good. Also a good website.

Jan B:
Thanks guys for all the replies. I feel instantly at home here at the forum!

I guess soldering is the more appropriate word for what i had in mind. Didn't quite figure it out yet what alloy these parts are made off. Can't find any reference for "monkey metal"  ;).
The alloy is mainly zinc with additions of magnesium, aluminum and copper. Often referred to as ZAMAK. Am i right?

I think i'll give it a try with Durafix, witch is available in the Netherlands.

Some of you pointed out the possibility of a fuel leak and the adherent risk of fire. Thanks for that. If a im not for 100% confident that its safe i will swap the bowl immidiatly.

And very generous of Menno to offer pre owned ones. I like that more than a new one because of the patina!


Cheers,

Jan

Bryanj:
"Monkey metal" is a generic term used here in UK to denote all the cheap, easily broken, unrepairable alloy mixes that are used. I believe, but willing to be proved wrong, that a high zinc content is part of it and carbs are cast from it. I tend to forget that English is a language that separates all the countries that speak it!

https://en.wikipedia.org/wiki/Pot_metal

K2-K6:
Agree with the above regarding zinc.

One of it's qualities I think is that the formation of zinc oxide on the surface is something like anodising aluminium,  a very thin and inert corrosion layer that makes it hard to stick anything to.  Normally on metal that has similar properties you have to flux them to get through this.

https://www.ebay.co.uk/i/122195024275?chn=ps&dispctrl=0&adgroupid=46846106558&rlsatarget=pla-384451231372&abcId=1128966&adtype=pla&merchantid=115165841&poi=&googleloc=9045909&device=t&campaignid=857332737&crdt=0&ul_ref=http%253A%252F%252Frover.ebay.com%252Frover%252F1%252F710-134428-41853-0%252F2%253Fmpre%253Dhttps%25253A%25252F%25252Fwww.ebay.co.uk%25252Fi%25252F122195024275%25253Fchn%25253Dps%252526dispctrl%25253D0%2526itemid%253D122195024275%2526targetid%253D384451231372%2526device%253Dt%2526adtype%253Dpla%2526googleloc%253D9045909%2526poi%253D%2526campaignid%253D857332737%2526adgroupid%253D46846106558%2526rlsatarget%253Dpla-384451231372%2526abcId%253D1128966%2526merchantid%253D115165841%2526gclid%253DEAIaIQobChMI6fLW___r1wIVS5PtCh1UogzJEAQYBSABEgJYR_D_BwE%2526srcrot%253D710-134428-41853-0%2526rvr_id%253D1381452946730

Above may offer a route if you and want to pursue soldering it.

Jan B:
I think you will have a laugh at me now....

The problem is that cup is very thin and heats up very quickly. The hole is near the hex shape at the bottom.Its much thicker there.

K2-K6 is right about the hard surface finish. Thats why you first lay dow a drop or two of liquid solder. Then you scratch with a stainless brush or something sharp in the liquid. Thus you break up the hard finish and the solder starts to bond with the "monkey metal". In this way there will be no re-oxidation of the surface because of lack of oxygen.

I've seen it done on carb parts on a classic event in the Netherlands. The solder is also called "Alutite".

I didn't make it that far because before the part with the hole became hot enough, the thin cup wall already melted. I should have applied the heat from underneath.

Lessons learned!

Cheers Jan