SOHC.co.uk Forums > Project Board

Another project ... a 400 four

<< < (3/7) > >>

dieffe:
Hi Oddjob,
The engine has been painted with Holts silver engine enamel, I hope it does last.
I shall remember to tighten the locknut up, cheers.

ST1100:

--- Quote from: dieffe on January 12, 2016, 09:25:16 PM ---I am zinc plating all the bolts that I can to save having to replace them but it is quite time consuming.
--- End quote ---
Nice work so far!
What procedure are you using for plating the engine bolts?

dieffe:
The zinc plating is done using one of those home plating kits, works well.

http://www.ebay.co.uk/itm/Zinc-Electroplating-Plating-Kit-for-Car-and-Bike-restoration-FREE-multimeter-/262180517329?hash=item3d0b2d35d1:g:5jYAAOxy1VlREOYU

ST1100:

--- Quote from: dieffe on January 13, 2016, 09:30:19 PM ---The zinc plating is done using one of those home plating kits, works well.
--- End quote ---
Durable? Or should one also peek at nickel plating? (more "bling" though, but maybe better corrosion protect...)

dieffe:
The zinc is ok if you passivate them with clear, blue or yellow. The nickel is better but more tricky to do.

Navigation